  • Incoloy a-286
  • Incoloy a-286
  • Incoloy a-286
  • Incoloy a-286
  • Incoloy a-286
Find Similar Products

Basic Info.

Model NO.
Incoloy A-286
Transport Package
in Spool, Carton, Wooden Case
Trademark
Ualloy
Origin
China
HS Code
75062000
Production Capacity
500 Tons/Year

Product Description

This age hardenable, Iron-Nickel-Chromium alloy is designed for applications requiring high strength and good corrosion resistance at temperatures up to 700oC (1290oF).
Chemical CompositionSpecificationsDesignationsKey FeaturesTypical Applications
ElementMin %Max %
C0.030.08
Mn1.002.00
Si-0.50
P-0.02
S-0.015
Cr13.5016.00
Ni24.0027.00
Mo1.001.50
Ti1.902.30
B0.0030.01
V0.100.50
Co-1.00
Al-0.35
Cu-0.50
Pb-0.005
AMS 5731
AMS 5734
AMS 5737
AMS 5853
ASTM A453
BS HR 52
BS HR 650
ISO 15156-3
(NACE MR 0175)
W.Nr 1.4944
W.Nr 1.4980
UNS S66286
AWS 023
High strength and good corrosion resistance at high temperatures
Age hardenable
Good for high temperature fasteners
High temperature static applications **
Jet Engines
Super Chargers
After Burner Parts
Fasteners
Density7.94 g/cm³0.287 lb/in³
Melting Point1430°C2600°F
Coefficient of Expansion16.4 μm/m °C (20 - 100°C)9.1 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity71.5 kN/mm²10370 ksi
Modulus of Elasticity205 kN/mm²29733 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy WireTypeTemperatureTime (Hr)Cooling
°C°F
Annealed or Spring TemperAge Harden705 - 7601300 - 140016Air
Properties
ConditionApprox. tensile strengthApprox. operating temperature
N/mm²ksi°C°F
Annealed600 - 75087 - 109-200 to +400-330 to +750
Annealed + Aged1100 - 1300159 - 188-200 to +400-330 to +750
Spring Temper1050 - 1250152 -181-200 to +400-330 to +750
Spring Temper + Aged1300 - 1500188 - 218-200 to +400-330 to +750

The above tensile strength ranges are typical. If you require different please ask.