Customization: | Available |
---|---|
Material: | Ni Cr |
Condition: | Bright, Annealed |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Chemical Composition | Specifications | Designations | Key Features | Typical Applications | |||||||||||||||||||||||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
|
ASTM B865 BS 3075 NA 18 BS 3076 NA 18 ISO 15156-3 (NACE MR 0175) QQ-N-286 |
W.Nr 2.4375 UNS N05500 AWS 041 |
Corrosion resistance similar to Monel 400 but with higher strength and hardness Low permeability and is non-magnetic to temperatures as low as -101°C (-150°F ) Age hardenable Good for sea water applications |
Pump Shafts Fasteners Marine Propeller Shafts Oil Well Tools Instruments Springs |
Density | 8.44 g/cm³ | 0.305 lb/in³ |
Melting Point | 1350°C | 2460°F |
Coefficient of Expansion | 13.7 μm/m °C (20 - 100°C) | 7.6 x 10-6 in/in °F (70 - 212°F) |
Modulus of Rigidity | 66 kN/mm² | 9573 ksi |
Modulus of Elasticity | 179 kN/mm² | 25962 ksi |
Heat Treatment of Finished Parts | |||||
---|---|---|---|---|---|
Condition as supplied by Alloy Wire | Type | Temperature | Time (Hr) | Cooling | |
°C | °F | ||||
Annealed | Age Harden Δ | 580 - 590 | 1075 - 1095 | 8 - 10 | Air |
Spring Temper | Age Harden Δ | 530 - 540 | 985 - 1005 | 4 - 6 | Air |
Properties | ||||
---|---|---|---|---|
Condition | Approx. tensile strength | Approx. operating temperature | ||
N/mm² | ksi | °C | °F | |
Annealed | 650 - 850 | 94 - 123 | -100 to +260 | -150 to +500 |
Annealed + Aged | 950 - 1050 | 138 - 167 | -100 to +260 | -150 to +500 |
Spring Temper | 1000 - 1300 | 145 - 189 | -100 to +260 | -150 to +500 |
Spring Temper + Aged | 1200 - 1500 | 174 - 218 | -100 to +260 | -150 to +500 |