• Hastelloy C-22
  • Hastelloy C-22
  • Hastelloy C-22
  • Hastelloy C-22
  • Hastelloy C-22
  • Hastelloy C-22

Hastelloy C-22

Product Type: Wire
Material: Ni Mo
Carbon Content: Low Carbon
Customization:
Shipping Cost:

Estimated freight per unit.

about shipping cost and estimated delivery time.
Payment Method: visa mastercard discover JCB diners club american express T/T
  Initial Payment Full Payment
Currency: US$
Return&refunds: You can apply for a refund up to 30 days after receipt of the products.
From payment to delivery, we protect your trading.
Hastelloy C-22 pictures & photos
Hastelloy C-22
US $33-38 / kg
Min. Order: 100 kg
Diamond Member Since 2012

Suppliers with verified business licenses

Secured Trading Service
Manufacturer/Factory & Trading Company

Basic Info.

Model NO.
Hastelloy C-22
Condition
Bright, Annealed
Transport Package
in Spool, Carton, Wooden Case
Specification
customized
Trademark
Ualloy
Origin
China
Production Capacity
500 Tons/Year

Packaging & Delivery

Package Size
50.00cm * 50.00cm * 40.00cm
Package Gross Weight
50.000kg

Product Description

 Hastelloy˘ C-22
Available in any of the 'profile options'
A Nickel-Chromium-Molybdenum alloy with better overall resistance and versatility than any other NiCrMo available. It has excellent resistance to localised corrosion and to a variety of mixed industrial chemicals.
Chemical Composition Specifications Designations Key Features Typical Applications
Element Min % Max %
Cr 20.00 22.50
Mo 12.50 14.50
Fe 2.00 6.00
W 2.50 3.50
C - 0.015
Si - 0.08
Co - 2.50
Mn - 0.50
V - 0.35
P - 0.02
S - 0.02
Ni Bal
ASTM B574
ASTM B575
ASTM B619
ISO 15156-3 (NACE MR 0175)
W.Nr 2.4602
UNS N06022
AWS 053
Better overall corrosion resistance than Hastelloy C-4 & C-276 and Inconel 625
Outstanding resistance to pitting, crevice corrosion and stress corrosion cracking
Chlorination systems
Nuclear fuel reprocessing
Pickling systems
Density 8.69 g/cm³ 0.314 lb/in³
Melting Point 1399°C 2550°F
Coefficient of Expansion 12.4 μm/m °C (20 - 100°C) 6.9 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity 78.6 kN/mm² 11400 ksi
Modulus of Elasticity 205.5 kN/mm² 29806 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 400 - 450 750 - 840 2 Air
Properties
Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 800 - 1100 116 - 159 -200 to +400 -330 to +750
Spring Temper 1400 - 1700 203 - 247 -200 to +400 -330 to +750

The above tensile strength ranges are typical. If you require different please ask.

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

From payment to delivery, we protect your trading.
Hastelloy C-22 pictures & photos
Hastelloy C-22
US $33-38 / kg
Min. Order: 100 kg
Diamond Member Since 2012

Suppliers with verified business licenses

Secured Trading Service
Manufacturer/Factory & Trading Company
Number of Employees
15
Year of Establishment
2012-02-06