Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t

Product Details
Customization: Available
Product Type: Strip
Material: Ni Cr Fe
Manufacturer/Factory & Trading Company

360° Virtual Tour

Diamond Member Since 2012

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Number of Employees
15
Year of Establishment
2012-02-06
  • Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t
  • Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t
  • Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t
  • Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t
  • Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t
  • Hot Sale Low Price 1.6mm SS316 Thermal Spray Equivalent to Tafa 85t
Find Similar Products

Basic Info.

Model NO.
SS316Ti
Condition
Bright, Annealed
Size
1.6mm,3.2mm
MOQ
One Spool
Packing
Wooden Case
Surface
Smooth
Transport Package
in Spool, Carton, Wooden Case
Trademark
Ualloy
Origin
China
HS Code
72230000
Production Capacity
800 Tons/Year

Product Description

316 Ti is similar to 316L but has better high temperature strength and mechanical strength.
Chemical Composition Specifications Designations Key Features Typical Applications
Element Min % Max %
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.50 18.50
Mo 2.00 2.50
Ni 10.50 13.50
Ti 5 x C 0.70
Fe bal
ASTM A240
ISO 15156-3 (NACE MR0175)
BS EN 10088-3
W.NR 1.4571
UNS S31635
AWS 168
Better corrosion resistance at higher temperatures than 316 stainless. Chemical processing.
Springs.
Fasteners.
Thread inserts.
Wire mesh.
Density 7.9 g/cm³ 0.285 lb/in³
Melting Point 1375°C 2500°F
Coefficient of Expansion 16.5 μm/m °C (21 - 100°C) 9.110 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity 74 kN/mm² 10730 ksi
Modulus of Elasticity 193 kN/mm² 27990 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 250 480 1 Air
Properties
Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 600 - 750 87 - 109 -200 to +300 -330 to +570
Spring Temper 1300 - 1600 189 - 232 -200 to +300 -330 to +570

The above tensile strength ranges are typical. If you require different please ask.

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier