High Temperature High Quality Alloy Hastelloy C-4

Product Details
Customization: Available
Product Type: Wire
Material: Ni Mo
Manufacturer/Factory & Trading Company

360° Virtual Tour

Diamond Member Since 2012

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Number of Employees
15
Year of Establishment
2012-02-06
  • High Temperature High Quality Alloy Hastelloy C-4
  • High Temperature High Quality Alloy Hastelloy C-4
  • High Temperature High Quality Alloy Hastelloy C-4
  • High Temperature High Quality Alloy Hastelloy C-4
  • High Temperature High Quality Alloy Hastelloy C-4
  • High Temperature High Quality Alloy Hastelloy C-4
Find Similar Products

Basic Info.

Model NO.
Hastelloy C-4
Carbon Content
Low Carbon
Condition
Bright, Annealed
Transport Package
in Spool, Carton, Wooden Case
Trademark
Ualloy
Origin
China
Production Capacity
500 Tons/Year

Product Description

Hastelloy˘ C-4
Available in any of the 'profile options'
This Nickel-Chromium-Molybdenum alloy tolerates high temperatures and gives a design freedom in areas where weld geometry makes excessive heat build-up unavoidable. Resistance to general and localised corrosion and stress corrosion cracking is generally similar to Hastelloy C-276.
Chemical Composition Specifications Designations Key Features Typical Applications
Element Min % Max %
Cr 14.00 18.00
Mo 14.00 17.00
Fe - 3.00
C - 0.015
Si - 0.08
Co - 2.00
Mn - 1.00
P - 0.04
S - 0.03
Ti - 0.70
Ni Bal
ASTM B574
ASTM B619
W.NR 2.4610
UNS N06455
AWS 052
Excellent resistance to stress-corrosion cracking and to oxidizing atmospheres at high temperature
Exceptional resistance to a wide variety of chemical process environments including, hot contaminated mineral acids, solvents, chlorine, formic and acetic acids, and salt waters.
Chemical processing
Density 8.64 g/cm³ 0.312 lb/in³
Melting Point 1399°C 2550°F
Coefficient of Expansion 10.8 μm/m °C (20 - 100°C) 6.0 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity 81.2 kN/mm² 11777 ksi
Modulus of Elasticity 212.4 kN/mm² 30807 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 400 - 450 750 - 840 2 Air
Properties
Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 800 - 1100 116 - 159 -200 to +400 -330 to +750
Spring Temper 1300 - 1500 189 - 218 -200 to +400 -330 to +750

The above tensile strength ranges are typical. If you require different please ask.