0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil

Product Details
Customization: Available
Product Type: Foil
Material: Feni
Still deciding? Get samples of US$ 10/Piece
Request Sample
Manufacturer/Factory & Trading Company

360° Virtual Tour

Diamond Member Since 2012

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Number of Employees
15
Year of Establishment
2012-02-06
  • 0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil
  • 0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil
  • 0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil
  • 0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil
  • 0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil
  • 0.08*160mm Feni42 4j42 Nilo42 Uniseal 42 Sealing Alloy Foil
Find Similar Products

Basic Info.

Model NO.
4J42
Carbon Content
Low Carbon
Certificate
ISO 9001&RoHS&BV
Chemical Composition
Fe, Ni
Size
Thickness:Less Than 0.05mm Width: Less Than 2
Usage
It Is Applied to Soft Glass-to-Metal and Ceramic-T
MOQ
50-100 Kgs Per Each Size; If We Have in Stock, 1kg
Payment
T/T, 30% Deposit and The Balance Paid Against The
Shippment
by Sea or by Air
Delivery Time
We Can Do The Order 45-50days Upon Receive The 30%
Advantages
1.Pass:ISO9001 Certification 2.Fine After-Sale Se
Status
Bright
Transport Package
According to Customer′s Requirements
Specification
RoHS, SGS
Trademark
Ualloy
Origin
Zhejiang, China
HS Code
87089910
Production Capacity
500tons/Year

Product Description


1.Description: 
 
 

Grade and chemical composition  

Grade

Mass fraction (%)

C

P

S

Mn

Si

B

Al

C0

Ni

Cr

Fe


4J42

0.05

0.020

0.020

0.80

0.30

 

0.10

1.0

41.5~42.5

 

balance

 
 
 

heat treating regime and coefficient of linear expansion

 

Grade

Heat treatment on samples

a/(10-6/K)

 

20-300°C

20~400%

20-450°C

 

4J42

Heat the sample to (900±20)°C in hydrogen atmosphere, keep the temperature for one hour, cool to below 200°C at the speed ≤5°C/min then discharge

4.0~5.0

 

6.5~7.5

 

6.5~7.2

6.5~7.2

 

 

9.2~10.0

9.2~9.9

 

 

 
 
 
 

coefficient of expansion  

 

Grade

Average coefficient of expansion a/(10-6/K)

 

20~100°C 

20~200°C 

20~300°C 

20~400°C 

20~450°C

20~500°C

20~600°C

 

4J42

5.6

4.9

4.8

5.9

6.9

7.8

9.2

 

 
 
 
 
2.Size
Foil:thickness:less than 0.05mm
     width: less than 200mm
 
 
 
3.Usage
It is applied to soft glass-to-metal and ceramic-to-metal seals in electronic component.
 
 
 
 
4.MOQ
 50-100 kgs per each size; If we have in stock, 1kgs is available for us.
 
 
5. Payment
 T/T, 30% deposit and the balance paid against the B/L copy.
 100% L/C at sight;
 Wesetern Union;
 Paypal;
 
6.Shippment
By Sea;
By Air (DHL,TNT,UPS,FEDEX etc)
 
 
7.Application
Petrochemical Industry;    Pulp and paper Industry;        Aerospace Industry;
Industrial Furnace;            Special Welding;                     Heating Treatment Industry;
Nuclear Power Industry;    Marine Industry;                       Shipbuilding Industry;
 
 
8.Packing
 Standard export packing, carton with plywood case for safety
Wire: below dia 1.0mm, packed in spool; Above 1.0mm, packed in coil
The goods can be packed as the clients demand.
 
 
 
9.Delivery time
We can do the order 45-50days upon receive the 30% deposit or L/C document.
 
 
 
10.Advantages
1.Pass:ISO9001 certification 
2.fine after-sale services 
3.small order accepted
 
11.Delivery conditions and finishes
 
 
 
Wire & coils: bright soft in oxidation condition; annealed soft wire ; half-soft bright wire
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier