Hastelloy C-2000

Product Details
Customization: Available
Product Type: Wire
Material: Ni Mo
Manufacturer/Factory & Trading Company

360° Virtual Tour

Diamond Member Since 2012

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Number of Employees
15
Year of Establishment
2012-02-06
  • Hastelloy C-2000
  • Hastelloy C-2000
  • Hastelloy C-2000
  • Hastelloy C-2000
  • Hastelloy C-2000
  • Hastelloy C-2000
Find Similar Products

Basic Info.

Model NO.
Hastelloy C-2000
Carbon Content
Low Carbon
Condition
Bright, Annealed
Transport Package
in Spool, Carton, Wooden Case
Trademark
Ualloy
Origin
China
Production Capacity
500 Tons/Year

Product Description

 Hastelloy˘ C-2000
Available in any of the 'profile options'
This alloy was developed to broaden the application range of one alloy. With the addition of Copper to the Nickel-Chromium-Molybdenum system, Hastelloy C-2000 is resistant to an extensive range of corrosive chemicals, including sulphuric, hydrochloric and hydrofluoric acids. The combination of Molybdenum and Copper provide excellent corrosion resistance to reducing media, while the high Chromium content gives good oxidising resistance.
Chemical Composition Specifications Designations Key Features Typical Applications
Element Min % Max %
Cr 22.00 24.00
Mo 15.00 17.00
Fe - 3.00
C - 0.01
Si - 0.08
Co - 2.00
Mn - 0.50
P - 0.025
S - 0.01
Cu 1.30 1.90
Al - 0.50
Ni bal
ASTM B574
ASTM B575
ASTM B619
W.Nr 2.4675
UNS N06200
AWS 055
Developed to resist corrosion in a wider range of media
Resistant to an extensive range of corrosive chemicals including sulphuric, hydrochloric & hydrofluoric acids
Superior pitting resistance and crevice corrosion resistance to Hastelloy C-276
Excellent corrosion resistance to reducing media
Good oxidising resistance
Chemical processing
Density 8.5 g/cm³ 0.307 lb/in³
Melting Point 1399°C 2550°F
Coefficient of Expansion 12.4 μm/m °C (20 - 100°C) 6.9 x 10-6 in/in °F (70 - 212°F)
Modulus of Rigidity 79 kN/mm² 11458 ksi
Modulus of Elasticity 206 kN/mm² 29878 ksi
Heat Treatment of Finished Parts
Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 400 - 450 750 - 840 2 Air
Properties
Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 700 - 1000 102 - 145 -200 to +400 -330 to +750
Spring Temper 1300 - 1600 189 - 232 -200 to +400 -330 to +750

The above tensile strength ranges are typical. If you require different please ask.